Fibers Give New 'Textile Concrete' Appeal

Wednesday, November 30, 2016

Comment | More

Fibers could be the key to a lighter, more durable and more versatile form of reinforced concrete, according to a new report from researchers at the Technical University of Dresden.

The team, led by civil engineer Manfred Curbach, has created what it calls “textile concrete,” which makes use of embedded carbon fibers to give it strength and stability instead of traditional steel reinforcement, according to German broadcaster Deutsche Welle.

German broadcaster Deutsche Welle shares an overview of the university's "textile concrete" material, including how it is made and the testing process.

In comparing its performance against steel-reinforced concrete, Curbach and his team see promising results, which they say will give engineers and designers an alternative tool when envisioning anything from residential structures and bridges to furniture and more.

Woven Mesh

Because carbon fiber is too soft on its own to be added directly to the concrete, Curbach explains that they need to be woven together and receive a coating to further stiffen them.

About 50,000 individual fibers are reportedly pulled together to form a yarn-like strand that is then woven into mesh on an automated loom before the layer of coating is added. The fibers are further adjusted in the weave, Curbach says, to give them “maximum tensility.”

The mesh is cut to size and placed between two millimeter-thin sheets of a special concrete mixture before the finished sheet is left to harden for 24 hours.

Robust Material, Slim Forms

Lab tests on a textile concrete girder have shown that even after cracks appear in the surface, the carbon material inside is able to withstand force to a level that makes it six times more robust than conventional steel-reinforced concrete, according to the team.

The team even built a test version of a bridge, which they loaded to the breaking point, Curbach says, so that authorities could see what the material could bear before granting approval for construction of the first textile concrete bridge.

Based on the knowledge gained from their research, the team sees great potential for carbon concrete. Whereas traditional concrete is “clunky and heavy,” Curbach says, the use of carbon creates slim elements instead.

Moreover, “Textile concrete costs less in terms of materials and energy used, so making it produces fewer emissions,” he adds.

   

Tagged categories: Asia Pacific; Building design; Building science; Coatings Technology; Colleges and Universities; Commercial / Architectural; concrete; EMEA (Europe, Middle East and Africa); Latin America; North America; Rebar; Research and development; Tensile strength

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Sauereisen, Inc.

 
SAFE Systems, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
DeFelsko Corporation

 
Fischer Technology Inc.

 
AWWA (American Water Works Association)

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us