If the walls of the Octagon Museum in Washington, D.C., could talk, they might tell tales of safekeeping the first lady’s pet parrot while the city was set ablaze by British troops, or perhaps recount the signing of the treaty that ended the War of 1812, or even recall the long-lost wallpaper that was once affixed in the entertaining rooms.

Octagon Exterior
Benjamin Moore & Company

A recent restoration project helped bring new life to the historic Octagon Museum in Washington, D.C.

The walls and the museum have witnessed some very significant pages in American history books and so keeping the structure in a restored state to share its story is paramount.

Recent restoration efforts to revive many of its historic finishes, mitigate its moisture and repair its original windows, further that goal.

Historic Home

The museum, designed by Dr. William Thornton, the original architect for the U.S. Capitol, was built in 1801 as a winter home for the Tayloe family of Virginia. In 1814, President James Madison and his wife, Dolley, lived in the house. (Dolley had sent her pet parrot to the Octagon for safekeeping when the British troops marched into Washington that year. President Madison also signed The Treaty of Ghent, which ended the War of 1812, at the Octagon on Feb. 17, 1815.)

Stair Hall
Benjamin Moore & Company

Walls in the museum were coated with period-appropriate finishes, based off of findings from a scientific paint layer analysis.

By the 1880s, the home had fallen into a state of neglect as it was being rented out by as many as 10 families. It was subsequently bought by the American Institute of Architects, and utilized as the organization's first national headquarters for many years.

Fast forward to today, the Octagon still stands—a free museum administered by the AIA Foundation. (The current AIA National headquarters building, constructed in the 1960s, is located directly behind the Octagon.)

Restoring that 1810 Look

The summer of 2016 was a refeshing time for the museum and its visitors, as many interior and exterior surfaces were repainted and restored, according to project details.

The painting project incorporated scientific paint analysis previously done on all the surfaces at the museum. The analysis was used to determine the precise colors on the walls when President Madison resided there.

Painting contractor Paintzen (New York) completed the recent project in about two months, according to the AIA Foundation. Benjamin Moore & Company donated all of the paint in period-correct colors.

A Wallpaper Mystery

Two rooms—the Treaty Room and Drawing Room—were unique in that the prior paint layer analysis revealed wallpaper glue from the 1810s, but no remnants of the wallpaper.

Though they first learned of the mystery wallpaper in the early 1990s, museum staff continue to research what the wallpaper might have looked like in the hopes that, one day,  a reproduction of the original can be produced and installed.

The Treaty room
Benjamin Moore & Company

The room above is where President James Madison, who lived in the house in 1814 and 1815, signed The Treaty of Ghent, which ended the War of 1812.

While the mystery remains unsolved, the museum decided to paint those rooms in period-appropriate shades selected from Benjamin Moore’s historic paint color collection. As it was one of the finest houses in the city, the original walls of the entertaining spaces would have incorporated bold colors of wall paint (and wallpaper) as a sign of wealth and status.

The walls of the Treaty Room were coated in a charcoal color as well as a denim shade of blue. Variations of a rose tone and red were used in the Drawing Room.

Drawing Room
AIA Foundation

Original walls of the Drawing Room, a room used for entertaining guests, would have been coated in bold colors to make a statement about wealth and status. The images show the Drawing Room before (left) and after (right) the paint project.

According to Benjamin Moore, the main challenge faced during the project was working in a museum that was both open to the public and full of 200+ year-old furniture.

The painters worked around tours and visitors enjoyed their “behind the scenes” peek at the progress.

Moisture Mitigation

The painting project followed an extensive moisture mitigation project that was completed in the fall of 2015.

Since it was first completed, the Octagon had been plagued with moisture issues, according to the museum. In a letter dated December 1814, Dolley complained about “dampness in the basement” during their stay at the Octagon.

moisture in walls
AIA Foundation

Moisture-damaged plaster has been removed from many basement surfaces. The museum staff must wait up to three years for the wall to dry before plaster can be reapplied.

In order to remedy the long-time issues, the rear foundation of the building was exposed and repairs and replacements were made to waterproofing there; all the drainage on the site was accessed and repaired/replaced as needed; and all basement window wells and areaways were re-waterproofed.

The site was also re-graded to ensure that water flowed away from the historic structure.

Additionally, moisture-damaged plaster was removed in many areas of the basement, including the kitchen and wine cellar.

The moisture-laden walls were then left to dry, according to the organization. Staff is continuously monitoring the moisture content and humidity levels in the basement.

“The drying is progressing, though slowly,” the organization wrote in project details, noting that it may be late 2017 or 2018 before new plaster can be reapplied to the basement walls.

The architecture firm Quinn Evans Architects (Washington) directed the moisture mitigation project and general contractor Corbett Construction (Virginia) completed the work.

Window Repairs

Also during that project, the museum’s original windows were “meticulously restored.” They were carefully stripped and repaired, and then re-glazed and repainted.

Windows AIAF
AIA Foundation

The historic windows were repaired and restored to their original glory.

Further, the pulley systems that historically allowed the windows to be opened and closed were also repaired; and reproduction hemp rope was used to hang the windows in a historically-correct manner.

Craftsmen Group (Maryland) played a key role in returning the windows to their original glory.

The Octagon is open from 1-4 p.m., Thursday through Saturday. Admission is free. Admiring the restoration is too.

   

Tagged categories: Aesthetics; American Institute of Architects (AIA); Architectural history; Benjamin Moore; Design; Historic Preservation; Historic Structures; Humidity and moisture; Maintenance + Renovation; Paint application; Project Photos; Renovation; Restoration; Waterproofing; Windows

Comment from Anna Rabinowitz, (10/31/2016, 9:04 AM)

Nice to see the continued restoration of the historic rooms. My first internship, while a historic preservation student in the mid 80's was to remove the many layers of paint rom the Coade stone mantlepiece and exposing the intricate pattern of the chair rails. It is nice to see that they are continuing the tradition of allowing visitors to view conservation in progress.


Comment from Tom Schwerdt, (10/31/2016, 9:06 AM)

That window frame being refurbished certainly had lead paint on it - some paint is still adherent, and there is apparent sanding/scraping debris on the work table, yet the worker has no respiratory protection and there does not appear to be a vent hood above the work. I wonder what his blood lead levels are, or if they were even tested.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Sauereisen, Inc.

 
HoldTight Solutions Inc.

 
Axxiom Manufacturing

 
Abrasives Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
Seal for Life/STOPAQ

 
CRW

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us