Wednesday, October 12, 2016

Comment | More

Researchers at one Singapore science and technology agency are looking at coating material microstructures in order to make protective coatings even tougher.

The team at A*STAR (Agency for Science, Technology and Research) has discovered how hard materials like chromium nitride—used as wear and corrosion protection coatings—behave when used in high-stress situations, the government agency reported Friday (Oct. 7).

This knowledge, they say, could lead to “producing even better coatings.”

Increasing Hardness

Resistance to wear can be improved by increasing a material’s hardness—that is, the force it can withstand before it begins to deform, A*STAR notes.

stressed out coatings
Photos: A*STAR Singapore Institute of Manufacturing Technology

Scanning electron microscope images show pristine (left) and compressed (right) micropillars of (top) chromium nitride, (middle) chromium aluminum nitride, and (bottom) chromium aluminum nitride/silicon nitride nanocomposite.

“In most crystalline materials, this deformation occurs when defects, known as dislocations, start to move through a material’s crystal structure,” the agency explains.

Materials used in coatings tend to be very brittle, they add. However, past research has shown that it can be very difficult to break crystals that are extremely small.

This inspired Shiyu Liu, and his team from the A*STAR Singapore Institute of Manufacturing Technology, to see how chromium nitride-based coatings deform under pressure.

Testing Deformations

After forming microscopic “pillars” of the materials, measuring about 380 nanometers across, they compressed the structures under a diamond flat punch in a scanning electron microscope at temperatures up to 500 degrees Celsius (932 degrees Fahrenheit).

The team found that chromium-nitride-based coatings made with very fine grains—i.e., those about 10 nanometers in size and separated by a thin grain boundary phase—withstood a much greater force before they deformed.

In fact, “deformation began at stresses very much higher than expected, and close to the theoretical maximum value from calculations,” the researchers report.

Liu's team explains that this increase in stress resistance became evident when the grains were so small they did not contain dislocations; as a result, the applied forces had to be sufficiently large to form new dislocations within the grains.

A*STAR research team

Of the team’s findings, A*STAR researcher Shiyu Liu (second from left) says, “This could be a viable approach for the development of super-hard and tough protective coatings for high-temperature and high-pressure applications.”

Moreover, the thin grain boundary phase was originally thought to be the main factor in determining the material’s properties, they note; however, their research demonstrates this was not the case. As a result, this can provide a way to reliably make a hard material, they add.

Next Stage

A*STAR reports that the team’s results show that the formation of a fine-grained microstructure could provide a ceramic coating with enhanced hardness and fracture toughness.

“This could be a viable approach for the development of super-hard and tough protective coatings for high-temperature and high-pressure applications,” says Liu.

The team plans to use the results in advanced manufacturing and engineering applications, such as protective coatings in high-speed machining tools for titanium and nickel-based alloys, the agency says.

The team’s research has been published recently in Scripta Materialia and Applied Physics Letters.

About A*STAR

Established in 1991, A*STAR is Singapore's lead government agency, housed under the Ministry of Trade and Industry of Singapore and dedicated to fostering world-class scientific research and talent for a vibrant knowledge-based economy.

   

Tagged categories: Asia Pacific; Coating chemistry; Coating Materials; Coating performance; Coatings Technology; Corrosion protection; EMEA (Europe, Middle East and Africa); Latin America; Nanotechnology; North America; Performance testing; Protective Coatings

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
DeFelsko Corporation

 
Tarps manufacturing, Inc.

 
AWWA (American Water Works Association)

 
Fischer Technology Inc.

 
SAFE Systems, Inc.

 
Modern Safety Techniques

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us