BASF Launches Sealant

Tuesday, August 9, 2016

Comment | More

A new sealant made to help accelerate construction project schedules and keep horizontal joints weathertight has been released by BASF.

MasterSeal SL 100 permits application to freshly placed (green) concrete as soon as 24 hours after forms are removed, compared to the 21 days recommended for most sealants, the company says. Enabling earlier access to jobsites allows contractors to save on labor costs, it explains.

Masterseal
BASF

The sealant is recommended for use on plaza decks, parking structures, balconies, industrial floors, driveways and garages, sidewalks, and numerous other horizontal joint applications.

Moreover, the sealant can also be placed on damp concrete, helping minimize the impact of rain on project schedules, according to the manufacturer.

Depending on weather conditions, the sealant can skin over between 5 to 45 minutes, which also helps shorten project schedules as this feature means it requires less time to dry and can reduce the accumulation of dust and debris, the company notes.

The sealant’s ability to adhere to substrates ranging from concrete and stone to metal means it can help simplify the sealant selection process, BASF says.

The company touts the sealant’s strong UV resistance, which contributes to a weather-tight seal that retains its color over time. The product can also be painted once it has cured, it adds.

Applications and Availability

Recommended uses include plaza decks, parking structures, balconies, industrial floors, driveways and garages, sidewalks, and numerous other horizontal joint applications.

Available in the U.S., Canada and Mexico, MasterSeal SL 100 is the newest product in the company’s MasterSeal line of sealants and waterproofing products, and part of BASF’s Master Builders Solutions brand.

It is available in easy-open, resealable packages, the company adds, helping to reduce material waste and labor.

More information: www.master-builders-solutions.basf.us.

   

Tagged categories: BASF; Coatings Technology; concrete; Floors; Parking Garages; Sealant; Waterproofing

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Sauereisen, Inc.

 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
Tarps manufacturing, Inc.

 
WEFTEC Show

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us