An established corrosion inhibitor for use in coatings and concrete admixtures is now available in liquid form.

Halox 570 LS, from ICL/ Advanced Additives (Hammond, IN), is a new liquid form of Halox 570, a powder corrosion inhibitor. The new form of the additive is designed to fight flash rust and galvanic corrosion, according to ICL.

Halox rust test
ICL/ Advanced Additives

Halox 570 LS is designed to fight flash rust and galvanic corrosion.

The manufacturer calls Halox 570 LS “environmentally friendly,” in addition to being nitrite-, phosphate- and heavy metal-free. It can be used in industrial or architectural coatings, and is recommended for water-based epoxy, acrylic or alkyd formulations, or concrete admixtures.

Adhesion and Gloss

Halox 570 LS is a standalone corrosion inhibitor, and is post-addable under agitation, according to ICL.

The powder version of Halox 570 is reportedly the company’s most widely used organic corrosion inhibitor. The liquid version, according to ICL, promotes adhesion and a high gloss finish for the coating.

More information: www.halox.com.

   

Tagged categories: Additives; Asia Pacific; Coating chemistry; Coating Materials; Corrosion inhibitors; EMEA (Europe, Middle East and Africa); Formulating; Latin America; North America

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Mitsubishi Gas Chemical America

 
NLB Corporation

 
SABRE Autonomous Solutions

 
DeFelsko Corporation

 
Tarps manufacturing, Inc.

 
SAFE Systems, Inc.

 
Fischer Technology Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us