New Coating Addresses Soapy Problem

Friday, July 15, 2016

Comment | More

Researchers behind a new technology say a new spray-applied coating will allow substances like soaps, which are built to stick, to slide right out of containers.

Coating test
Image from video by Philip S. Brown, courtesy of The Ohio State University

Researchers say they have developed a superoleophobic lining for shampoo bottles and other applications.

Philip S. Brown and Bharat Bhushan, from The Ohio State University, have published a paper in Philosophical Transactions of the Royal Society A, purporting to have developed the new technology.

Silica Nanoparticles

The trick, the team explains, involves silica nanoparticles, spray-applied to the plastic surface using a solvent. The substance in the bottle can’t get a grip on the plastic surface, because the silica particles are guarding it. The soap can’t seep between the particles, and air pockets form between them, underneath the soap—that’s what keeps the soap moving along.

It’s nice for consumers, and might save them a few bucks, but it’s also big business: “Manufacturers are really interested in this, because they make billions of bottles that end up in the garbage with product still in them,” said Bhushan, a professor of mechanical engineering at Ohio State.

The coating is designed specifically to work on polypropylene, known in the United States as “number 5” plastic.

From Food to Soap

Other products have addressed the same problem in different ways. A nonstick nanocoating barrier for food applications was developed at Massachusetts Institute of Technology in 2012 and hit the consumer market last year, promising to let you get ketchup out of the bottle more easily. That substance has been licensed for use in food products in Europe.

The soap issue is a stickier subject, though.

“Compared to soaps, getting ketchup out of a bottle is trivial,” Bhushan says. “Our coating repels liquids in general, but getting it to repel soap was the hard part.”

   

Tagged categories: Coatings Technology; Colleges and Universities; Nano and hybrid coatings; Nanotechnology; Research and development

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Induron Coatings, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Mitsubishi Gas Chemical America

 
Tarps manufacturing, Inc.

 
SABRE Autonomous Solutions

 
RCG America

 
Fischer Technology Inc.

 
DeFelsko Corporation

 
Modern Safety Techniques

 
NLB Corporation

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us