Air Barriers Get Revamp

Wednesday, June 8, 2016

Comment | More

New formulations of two air and waterproof barriers mean easier application, according to the products’ manufacturer.

R Guard being applied
Prosoco

The two liquid-applied barriers have both been reformulated, Prosoco says, so that they’re easier to roll on than in the past.

R-Guard Cat 5 and R-Guard Cat 5 Rain Screen, liquid-applied barriers from Prosoco Inc., have both been reformulated, the company says, so that they’re easier to roll on than in the past. Prosoco notes that this will be especially noticeable in low-temperature application situations.

About the Products

R-Guard Cat 5 is described as a one-component air and waterproof barrier that creates a seamless elastomeric weatherproofing membrane. R-Guard Cat 5 Rain Screen is an air and water-resistive barrier, for use in the construction of rain screens.

Both products are solvent-free, isocyanate-free and phthalate-free, and are touted as capable of standing up to the heavy rains and 155 mph winds of a Category 5 hurricane.

Faster Cure Time

Prosoco notes that in addition to improved rheology, the new formulation offers a quicker cure time than in the past.

According to Prosoco, both products cure in wet conditions and on damp substrates.

The products can be used in conjunction with previous formulations.

For more information: www.prosoco.com.

   

Tagged categories: Air barriers; Building Envelope; North America; Prosoco Inc.; rain screen design; Waterproofing

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
WEFTEC Show

 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us