In a recent study, Canadian researchers reported the ability to calm a chemical reaction that has traditionally caused glass-fed concrete to weaken, expand and crack, a reaction known as “concrete cancer.”

The team from the University of British Columbia Okanagan campus reports it has found a more reliable way to make concrete from discarded glass, the university announced Wednesday (May 25).

UBC
UBC

UBC's Anant Parghi (left) and Associate Professor Shahria Alam with a piece of "green" concrete and some of the glass that helped make it.

The findings were recently published in the journal Construction and Building Materials.

A Step Forward

“Every year, millions of tons of glass bypass recycling centres and end up in North American landfills,” explained Associate Professor of Engineering Shahria Alam. “Like many engineers, we are interested in making smarter building materials that can give the construction industry the resources they need without necessarily having to take new resources out of the ground.”

Alam said that researchers have been on the lookout for ways to reliably make use of glass in concrete construction. He said his team’s research represents a significant step forward in the search.

Concrete cancer occurs when the alkaline properties in cement paste react with silica properties that can occur in recycled concrete additives, such as glass, the university reports.

Study Details

In their study, Alam and co-researcher Anant Parghi discovered that by adding a water-based, synthetic rubber polymer, fly ash, and silica powder to the concrete mixture, they were able to effectively neutralize negative chemical reactions.

“By partially replacing cement with polymer, fly ash and glass powder, we were able to produce concrete that was more than 60 percent stronger than what was previously believed possible,” said Parghi. “Though further testing is needed to assess long-term stability, it now looks like we can replace up to 25 percent of the cement materials that had to be mined for cement production with glass.”

All of the glass used in the study was taken from the landfill in Kelowna, BC, and was considered waste at the time it was retrieved. The concrete additives were donated from Kelowna-based company POLYRAP Engineered Concrete Solutions.

   

Tagged categories: concrete; Concrete defects; Construction; Cracks; Glass; Good Technical Practice; Recycled building materials; Research and development

Comment from Tom Schwerdt, (6/7/2016, 12:22 PM)

"Concrete Cancer" - what a clickbait, worthless term. Are they actually talking about ASR? It's been known for a long time that substituting Class F fly ash for some of the cement allows you to use a more reactive aggregate. Additionally, I find it hard to believe that somehow their mix is producing concrete 60% stronger (compression? tensile? Flex?) than Ultra high performance concrete, since we know UHP concrete performance is quite possible.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
WEFTEC Show

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us