A new high-performance floor topcoat said to resist yellowing over the long term is now available from Coatings for Industry Inc. (Souderton, PA).

Wearcoat 481HP is described as a 100 percent solids, light stabilized, self-leveling epoxy floor coating. The company says it offers very good chemical resistance properties, zero volatile organic compounds, extremely low odor and a wide range of film thicknesses.

Anti-Yellowing Properties

The new epoxy coating was reportedly designed as an upgrade from the company’s Wearcoat 440 for applications where the floor has exposure to damaging sunlight or high-intensity lighting. 

Coatings For Industry

The new high-performance epoxy topcoat from Coatings For Industry boasts anti-yellowing and fade-resistant properties, said to make it ideal for settings subject to damaging sunlight or high-intensity lighting.

It was formulated from the start to be both anti-yellowing and fade-resistant, solving a problem common to conventional epoxy coatings, according to the industrial coatings manufacturer.

While all epoxies will eventually yellow, the company claims it will take twice the exposure for its new topcoat to change noticeably, and adds that it also improves wear resistance by 30 percent over conventional epoxy flooring. 

“The 481HP has been in development for some time, and we’re excited to make it available,” says Kevin Klotz, president of CFI. 

“Anti-fade, anti-yellow has been one of the holy grails in epoxies,” he adds. “Both accelerated exposure testing in our lab and field results leave us confident this will be a game changer.”

Recommended Applications

Appropriate for indoor and outdoor applications, the company says its extensive testing has demonstrated that it should prove ideal for garages, hangars or other areas exposed to UV rays.

According to the manufacturer, the topcoat is especially effective in providing a seamless floor with good resistance to an array of hazards, such as those encountered in aircraft hangars or emergency and medical facilities. 

It also suggests that the system is ideal for application at facilities that are in service because it has zero VOCs and extremely low odor. 

All of the decorative options available for Wearcoat 440, including flakes, quartz and metallics, are also available for the new Wearcoat 481HP. It is available as 1 gallon and 5 gallon kits.

More information: www.cficoatings.com.

   

Tagged categories: Asia Pacific; Coating Materials; Coatings; Coatings for Industry Inc.; Coatings Technology; EMEA (Europe, Middle East and Africa); Epoxy; Fade-Resistant Color; Floor coatings; Latin America; Low odor; North America; Topcoats; UV resistance; VOC-free; Zero-VOC

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
HoldTight Solutions Inc.

 
Strand’s Industrial Coatings

 
NLB Corporation

 
Tarps manufacturing, Inc.

 
REMA Corrosion Control

 
CRW

 
Modern Safety Techniques

 
Paint BidTracker

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us