SSPC: New Wet Abrasive Blast Standards

Thursday, March 31, 2016

Comment | More

Five new joint SSPC-NACE Wet Abrasive Blast Cleaning standards are now available from SSPC: The Society for Protective Coatings.

Wet abrasive blast (WAB) cleaning is primarily specified for suppression of dust in areas that would otherwise be prepared by dry abrasive blast cleaning, the association explains.

wet abrasive blasting
Photos: Rescue 1 via r4r7r9

SSPC recently released five new joint SSPC-NACE Wet Abrasive Blasting Standards.

An additional benefit of using wet surface preparation methods is that they will reduce the levels of any non-visible water-soluble contaminants, such as soluble salts, that may be present on the surface and adversely affect coating performance, it adds.

Although the definitions of surface cleanliness immediately prior to coating application are the same for both the WAB and dry abrasive blast cleaning standards, the association says, the wet abrasive blast cleaning standards eliminate the need for “customizing” the dry blast cleaning standards to address flash rust levels and other specialized equipment and procedures that must be used with wet cleaning methods.

The newly published joint standards are:

The standards are intended for use by coating or lining specifiers, applicators, inspectors or others whose responsibility is to define a standard degree of surface cleanliness for carbon steel surfaces to be achieved by wet abrasive blast cleaning.

Technical Content

These standards combine elements of the existing standards for dry abrasive blast cleaning with elements of the 2012 SSPC/NACE waterjet cleaning standards, according to SSPC. 

The definitions of cleanliness for the steel surface immediately following wet abrasive blast cleaning are identical to the definitions in the five dry abrasive blast cleaning standards. However, because water is used to convey the abrasive onto the surface, a layer of flash rust will form on the cleaned steel as the water evaporates, the association explains. 

Due to the varied tolerance of coatings for the presence of flash rust on the surface, contractors must know the maximum permissible level of flash rust that may be present on the steel immediately prior to the application of the protective coating, as well as how to assess how much flash rust has developed.

The WAB cleaning standards define four levels of flash rust: no flash rust, light flash rust, medium flash rust, and heavy flash rust. 

These definitions are based on the extent to which the flash rust obscures the underlying steel substrate, the ease with which it can be removed by wiping with a cloth, and the amount of material that appears on the cloth after the surface is wiped, SSPC says.

wet abrasive blast cleaning

The new joint standards combine elements of the existing standards for dry abrasive blast cleaning with elements of the 2012 SSPC/NACE waterjet cleaning standards, SSPC says.

As with the waterjetting standards and the dry abrasive blast cleaning standards, the association adds, the WAB cleaning standards also include information on materials and methods used to perform the cleaning process.

For example, the water used must be free of contaminants that would affect the cleanliness of the prepared surface and the functioning of the pumps or other equipment. If the project specification includes specific requirements for non-visible contaminants, the water used for waterjetting must be free of impurities that could prevent the surface from meeting those requirements.

Training Compatibility

SSPC notes that the new WAB standards are relevant to the following SSPC Training and Certification Programs as well:

  • Abrasive Blasting Program (C7)
  • Basics of Estimating Industrial Coatings Projects (EST)
  • Basics of Steel Surface Preparation eCourse
  • Bridge Coatings Inspector Program (BCI)
  • Bridge Maintenance: Conducting Coating Assessments (BRIDGE)
  • Coating Application Specialist Certification Program (CAS)
  • Coating Application Specialist Refresher (CAS REF)
  • Developing an Effective Coating Specification (DEV CTG SPEC)
  • Fundamentals of Protective Coatings (C1)
  • Lead Paint Removal (C3)
  • Lead Paint Removal Refresher (C5)
  • Lead Paint Worker Safety (WORKER)
  • Master Coatings Inspector Certificate (MCI) 
  • Navigating NAVSEA Standard Item 009-32 (009-32)
  • NAVSEA Basic Paint Inspector (NBPI)
  • Planning and Specifying Industrial Coatings Projects (C2)
  • Plural Component Application for Polyureas and High Solid Coatings (PLURAL)
  • Project Management for the Industrial Painting Contractor (PRO MGMT)
  • Protective Coatings Inspector Program (PCI)
  • Protective Coatings Specialist (PCS) Program
  • Quality Control Supervisor (QCS)
  • Water Jetting Program (C13)

More information: http://www.sspc.org/.   

   

Tagged categories: Asia Pacific; Certifications and standards; EMEA (Europe, Middle East and Africa); Latin America; NACE; North America; SSPC; Surface Preparation; Wet abrasive blasting

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
Strategic Materials Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us