Scientists Bind Metal to Metal Sans Heat

Tuesday, January 26, 2016

Comment | More

Nanotechnology experts from Northeastern University in Boston say they have a developed an adhesive that binds metal to metal, sets at room temperature and requires little pressure to seal.

“It’s like welding or soldering but without the heat,” Hanchen Huang, professor and chair in the Department of Mechanical and Industrial Engineering at Northeastern, said in a recent announcement on the development.

Huang and his team say the metallic glue, called MesoGlue, has an array of potential applications, including solar cells, pipe fittings and components for computers and cell phones.

The team has published their findings in the January issue of Advanced Materials & Processes.

Fortune Magazine reports that the coating is in a class of its own, suggesting that the development may be the “21st Century’s Duct Tape.”  

“Until now, adhering metal to metal has been a difficult, messy process or required soldering—fusing two parts together with a hot metal joint,” the media outlet reports. “Room temperature glues can’t really compete with this method: They don’t conduct electricity and many break down in heat.”

How it Works

MesoGlue is a based on a system of “metal-cored nanorods” coated with a layer of liquid metal elements like indium and gallium.

“When those outer layers of elements are pushed together during gluing they interact with the nanorods inside the glue and turn solid, no heat required,” reports Fortune.

Solar panel
©iStock.com / Tverdohlib

In addition to computers and cell phone components, applications include solar cells.

The resulting glue provides the strength and thermal/electrical conductance of a metal bond, Northeastern University reports.

The researchers said they have received a new provisional patent for the development through Northeastern.

Inspiration

Inspiration behind the development came from the desire to make dye-sensitized solar cells last longer, according to Mesoglue.com.

The developers soon realized the adhesive could have other uses.

“We then heard reports of iPhones exploding, and realized that not only could we make devices safer, but could make them run cooler and last longer as well.”

MesoGlue was founded by Huang and two of his Ph.D. students who had “a dream of a better way of sticking things together.”

   

Tagged categories: Adhesive; Coating chemistry; Coatings Technology; Metallic coatings; Metals; Nanotechnology; North America; Research

Comment from Tom Schwerdt, (1/26/2016, 8:46 AM)

Calling this equal in strength to a metal bond is a stretch. In the linked article, it's only a 1500 PSI bond. You can readily get metal filled conductive epoxies that cure at room temperature with higher strength. Took me maybe 15 seconds on Google to find one with 2000 psi. "Without the heat" is also a stretch - to minimize voids for the thermal conductivity comparison, the researchers used a 100C application temperature (boiling water). Is this technology interesting? Sure. Needs more detail on conductivity (thermal and electrical) as well as heat/thermal cycling resistance since those are touted benefits. Outperforming Arctic Silver 5 thermal paste for a test on a real CPU was very intriguing. I would need to see reproducibility from elsewhere, as AS5 performance can be dramatically reduced by poor application. Not much of a concern for a production environment once you have the process down, but new users often have to practice to get the application method down.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
WEFTEC Show

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us