Coating to Aid in Water, Dirt Repel

Thursday, December 3, 2015

Comment | More

University of Massachusetts scientists say they have come up with a process for making transparent coatings that will help repel water and dirt from various substrates.

The process, as noted in Nanowerk News, could help formulators manufacture coatings that would make graffiti removal easier, for example. Unlike current processes, the researchers said, the newly developed system causes liquids to bead up and slide off, similar to the mechanisms of a lotus blossom.

The team published its findings in the journal Angewandte Chemie.

The paper, “Covalently Attached Liquids: Instant Omniphobic Surfaces with Unprecedented Repellency,” describes the process for the production of SOCAL (slippery, omniphobic, covalently attached liquid) surfaces.

©iStock.com / Totojang

Researchers at the University of Massachusetts have developed an omniphobic coating process that they say will make creation of a transparent coating to repel water and dirt easier.

Researchers Liming Wang and Thomas J. McCarthy said that glass slides using their method can be coated in minutes by dipping them in the solution, letting them dry and then rinsing them.

They state that the omniphobic coating can repel any kind of liquid.

Chemical Components

The solution contains a siloxane monomer (Me2Si(OMe)2) and sulfuric acid in isopropanol, according to Nanowerk. When an object is dipped into the liquid, a thin film of liquid forms on the surface and creates a polymer as it dries. Polydimethylsiloxane (PDMS)—a biocompatible silicone oil used in medical applications—chains form and are anchored to the surface as it is catalyzed by the sulfuric acid.

The coating is homogenous, and being so, is important for omniphobicity, noted Nanowerk. Aqueous and organic liquids reportedly roll off of coated slides without leaving a trace, even at a minimal angle of inclination.

The PDMS chains can move around as though they were in a liquid, the report said. Hexane rolls off at an incline of 1 inch, even though its surface tension is less than that of PDMS. The coatings are thermally stable and show omniphobic properties even after a year in storage, the report suggests.

   

Tagged categories: Coating chemistry; Coatings Technology; Dirt resistance; Graffiti resistance; Nanotechnology; North America; Research; Water repellents

Comment from Mark Jones, (12/3/2015, 7:10 AM)

"similar to the mechanisms of a lotus blossom"-? Thought STO already did this "bio-mimicry" with their Lotusan. Pretty amazing coating technology.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
SABRE Autonomous Solutions

 
DeFelsko Corporation

 
Mitsubishi Gas Chemical America

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
Induron Coatings, Inc.

 
RCG America

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us