Cardolite Corporation has debuted an epoxy curing agent for commercial use, including concrete coatings and grouts, mortars and adhesives.

Lite 3025 builds on the cashew nutshell liquid (CNSL) curing technology developed previously for the Lite 3000-series agents, the company says. The new solvent-free agent is formulated for cost-effective, medium and high solids heavy duty epoxy coatings, according to Cardolite.

©iStock.com / jkitan

The Cardolite Lite 3025 is a CNSL phenalkamide epoxy curing agent that the company said can be used for concrete coatings, grouts, mortars and adhesives.

According to Cardolite, CNSL curing agents with phenalkamine are used in the heavy-duty coatings market because of their corrosion protection qualities, mechanical strength and fast cure rate, even at low temperatures.

The company's proprietary CNSL technology modified with a phenalkamine, called phenalkamide, offers the same protection but improves on similar product drawbacks such as color, overcoat window, and flexibility that have prevented a wider application use, the company said.

The product has "drop in" compatability with existing epoxy systems to avoid the time and costs associated with reformulation, according to the company.

More information: www.cardolite.com.

   

Tagged categories: Adhesive; Asia Pacific; Coating chemistry; Coatings Technology; Coatings Technology; Concrete coatings and treatments; Curing; EMEA (Europe, Middle East and Africa); Epoxy; Grout; Latin America; Mortars; North America

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
EDCO - Equipment Development Co. Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us