Extrusion Coatings Made to Sparkle

Tuesday, November 3, 2015

Comment | More

Valspar Corp. has introduced a new line of architectural coatings billed to offer deep color hues and intense sparkle.

The Nova color line is a 70 percent polyvinylidene difluoride (PVDF) coating that can be matched to nearly any color, according to the company. Part of the Fluropon Effects family, Nova is available for coil and extrusion applications and meets AAMA 620, 621 and 2605-13.

Valspar

The Nova color line is a 70 percent polyvinylidene difluoride (PVDF) coating that can be matched to nearly any color and retain hue and sparkle, according to Valspar.

Nova is available with a gold or silver sparkle finish, Valspar said. The company also said the resin-based coating has good color and gloss retention; stands up well to weathering; and is resistant to dirt, stains, chalking and fading.

Valspar said the product is being tested on aluminum extrusions; mullions; soffits and fascia; aluminum-framed windows; entrances; skylights and curtainwall; metal roofing systems; and composite and insulated metal wall panel systems.

More information: www.valsparglobal.com.

   

Tagged categories: Aluminum; Architectural coatings; Asia Pacific; Coating selection; Coil Coatings; Curtain wall extrusions and cladding; Decorative Finishes; EMEA (Europe, Middle East and Africa); Extrusions; Latin America; North America; PVDF; Roof coatings; Valspar

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
Strand’s Industrial Coatings

 
Sauereisen, Inc.

 
CRW

 
Paint BidTracker

 
Modern Safety Techniques

 
HoldTight Solutions Inc.

 
NLB Corporation

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us