The Garland Company Inc. has introduced a new commercial roofing system designed to increase its resiliency as it ages.

The OptiMax roof system uses a thermoset polyurethane-modified membrane to achieve its resiliency, according to the company. The technology that Garland uses combines asphalt and polyurethane to help prevent cracking and leaking, the company said.

Garland

Billed as an industry first, the OptiMax roof system uses a thermoset polyurethane-modified membrane to achieve its resiliency, according to Garland.

Garland said the mixture of asphalt and polyurethane also helps improve mineral adhesion and provides good UV protection. During surface testing, OptiMax had fewer cracks compared to traditional asphalt-modified membranes and retained its tensile strength when exposed to UV radiation, the company said.

The new roof system also stands up well against heat and chemicals, the company said.

More information: www.garlandco.com.

   

Tagged categories: Asphalt; Building Envelope; Building envelope; Commercial / Architectural; Commercial Construction; Garland Company; North America; Polyurethane; Roofing materials

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
HoldTight Solutions Inc.

 
CRW

 
Tarps manufacturing, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Seal for Life/STOPAQ

 
Abrasives Inc.

 
Axxiom Manufacturing

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us