A team of researchers has developed a polymer-based material that changes color depending on the strength of impact.

The team's vision is to see the technology used to give a clear, visual indication of dangerous head injuries when used in protective headgear.

The Basis of the Research

Diagnosing whether someone has suffered head trauma at the time of an accident—whether for a player on the football field or a soldier near a bomb blast—is not a fast or easy process.

But a product that immediately changes color depending on how hard it is hit could help provide immediate detection of a serious head injury.

“If the force was large enough, and you could easily tell that, then you could immediately seek medical attention,” said Shu Yang, Ph.D. in a release from the American Chemical Society (ACS).

American Chemical Society

A research team at the University of Pennsylvania is working on a polymer material that changes color based on impact force in order to help in the quick identification of serious head injuries.

According to ACS, Yang’s team at the University of Pennsylvania used holographic lithography (HL) to create photonic crystals with structures carefully designed to give them a particular color, like an opal.

When a force as applied, the crystals’ internal structures changed and became deformed, changing the color.

Deforming the crystals with an applied force changed their internal structures, and also the crystal’s color, enabling medical personnel to readily identify damaging force on-site without additional tools.

Adapting the Process

The HL method of making these crystals is expensive, however, making it unsuitable for mass production, Yang said.

Her team opted for self-assembly and polymer-based materials that are cheaper to produce over a large area than the original HL method and, according to Younghyun Cho, Ph.D., a postdoctoral fellow in Yang’s lab, this adjusted procedure could be the path to commercialization.

In the new approach, they molded the polymer into a structure that worked in the same ways the photonic crystals did.

They tested the polymer material with the application of various levels of force and recorded the color change, seeing the results they were looking for.

 “We were able to change the color consistently with certain forces,” Yang said.

For example, with the approximate force of a sedan moving at 80 miles per hour crashing into a brick wall, the material changed from red to green. With a force equal to a speeding truck hitting the wall, they polymer turned purple, said Cho.

The polymer the team developed changes different colors based on the force of impact, which helps to indicate if it was strong enough to cause concussion.

“This force is right in the range of a blast injury or a concussion,” said Yang.

It is unclear whether the polymer material will continue to be molded or applied via another method.

In future studies, Yang said she plans to develop materials that can indicate how quickly a force is applied, which affects how damaging a particular trauma is on the brain.

Her team presented their research at the 250th National Meeting & Exposition of the ACS. The ACS is a nonprofit organization chartered by the U.S. Congress, the world’s largest scientific society, and a global leader in providing access to chemistry-related research.

   

Tagged categories: American Chemical Society; Asia Pacific; Coating chemistry; Coating Materials; EMEA (Europe, Middle East and Africa); Latin America; North America; Polymers; Research and development

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
CRW

 
Abrasives Inc.

 
Axxiom Manufacturing

 
Sauereisen, Inc.

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
GMA Garnet USA

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us