Glass Paint Designed to Cool Roofs

Wednesday, August 19, 2015

Comment | More

From metal roofs to naval ships, a novel coating can supposedly keep surfaces at air temperature under the sun and help prevent premature aging.

The glass-based, environmentally friendly coating is being developed by Jason J. Benkoski, Ph.D., senior scientist in the Johns Hopkins University Applied Physics Lab.

Inspired by Glass

Benkoski says he chose to work with glass, which is made out of silica, for the coating because it is hard, durable and has the right optical properties.

glass coating testing tiles
American Chemical Society

Benkoski's silica-based coating, for use on military ships and other metal surfaces, can expand and contract with fluctuating air temperatures, reflect sunlight and resist water.

He told Forbes magazine, his lab was inspired by the durability of paints known as “water glass.”

“The starting materials are the cheapest things you can imagine—sand and potash,” he said.

The long-standing facades in Germany and Switzerland were given as an example of the exterior use of water glass paints—they likely have maintained their splendor over time because the glass reflected sunlight.

Water glass paints required a clean rough surface to cling to, though, which doesn’t make them a good match for metal, Benkoski explained. 

In the Lab

In the lab, Benkoski began with silica, one of the most abundant materials in the Earth’s crust, and modified one version of it, potassium silicate, that normally dissolves in water. His tweaks transformed the compound so that when it’s sprayed onto a surface and dries, it becomes water resistant.

Benkoski explained the logic behind his research: “Most paints you use on your car or house are based on polymers, which degrade in the ultraviolet light rays of the sun. So over time you’ll have chalking and yellowing.

“Polymers also tend to give off volatile organic compounds, which can harm the environment. That’s why I wanted to move away from traditional polymer coatings to inorganic glass ones,” he said in a release from the American Chemical Society.

Benkoski reflectance testing
American Chemical Society

This silica-based coating is designed to keep an outdoor metal surface close to air temperature and thereby slow down corrosion and other types of degradation.

Unlike acrylic, polyurethane or epoxy paints, Benkoski’s paint is almost completely inorganic, which should make it last far longer than its counterparts that contain organic compounds, according to the ACS. His paint is also designed to expand and contract with metal surfaces to prevent cracking.

Mixing pigments with the silicate gives the coating an additional property: the ability to reflect all sunlight and passively radiate heat. Since it doesn’t absorb sunlight, any surface coated with the paint will remain at air temperature, or even slightly cooler. That’s key to protecting structures from the sun.

“When you raise the temperature of any material, any device, it almost always by definition ages much more quickly than it normally would,” Benkoski said.

“It’s not uncommon for aluminum in direct sunlight to heat 70 degrees Fahrenheit above ambient temperature. If you make a paint that can keep an outdoor surface close to air temperature, then you can slow down corrosion and other types of degradation.”

“It’s almost like painting a rock on top of your metal. And this is going to last not tens of years but maybe hundreds of years,” he said in National Geographic.

Applications in the Field

The paint Benkoski’s lab is developing is intended for use on naval ships (some funding for his work was provided by the U.S. Office of Naval Research), but it has other potential commercial applications, including as a cool roof coating.

“You might want to paint something like this on your roof to keep heat out and lower your air conditioning bill in the summer,” he said.

“White paint by itself does a good job,” reflecting about 90 percent of the sun’s energy, he told National Geographic.

But, he explained, a polymer-based coating cannot reject ultraviolet light like a silica-based paint can. “With as little as three years of UV degradation, a polymer paint could absorb twice as much solar energy as it did when freshly painted,” he added.

Mixing pigments with the silicate gives the coating the ability to reflect sunlight and passively radiate heat.

He suggested the paint could also go on metal playground slides or bleachers. And it would be affordable. The materials needed to make the coating are abundant and inexpensive.

He indicated he also expects to find applications for ceramics such as glass, concrete and rock, as well as fiberglass or previously polymer-painted surfaces.

Development Schedule

Not yet on the market, Benkoski says he expects his lab will start field testing the material in about two years.

He told National Geographic it could take five years for the product to reach the commercial market, and he expects the paint’s chances for success will be bolstered by the Navy’s sponsorship of his research.

Benkoski presented his work at the 250th National Meeting & Exposition of the American Chemical Society (ACS) on Sunday (Aug. 16). ACS, the world’s largest scientific society, is holding the meeting in Boston through Thursday (Aug. 20).

   

Tagged categories: Coating chemistry; Coatings Technology; Coatings Technology; Cool roof coatings; Corrosion resistance; Laboratory testing; North America; Protective Coatings; Reflectance; Reflective coatings; Reflective roof coatings; Research and development; Solar reflectance

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
WEFTEC Show

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us