Coatings Industry News

Main News Page


Study: White Roofs Keep the Temp Down

Wednesday, July 29, 2015

Comment | More

Researchers at Queensland University of Technology have discovered that a certain reflective, white coating can decrease a building’s inside temperature when it’s applied to the roof.

The paint led to a 2-degree Celsius (3.6-degree Fahrenheit) drop in temperature to the inside areas, according to the study.

Study Details

The two-year project was led by professors John Bell, head of the School of Chemistry, Physics and Mechanical Engineering; and Wendy Miller, a senior research fellow at the school in Brisbane, Australia.

They looked at how the coating affected 16 buildings on 10 sites without air conditioning, and then took measurements both before and after applying the special white coating. The researchers then checked the temperature on the roof surface, on the roof cavity and on the inside of the structures.

Not only did the coating lower the temperature, it lowered electric bills, too.

Queensland University of Technology/Erika Fish

Queensland University of Technology researchers John Bell and Wendy Miller have found that a roof with a special reflective white coating can lower the inside temperature and cut electricity bills.

“We saw average energy savings of between 5 (percent) and 30 percent across the range of buildings, with most buildings showing savings above 15 percent," said Bell of the findings.

“For an air-conditioned block of two classrooms in Springfield to the west of Brisbane, for example, we reduced electricity use by 1,144 kilowatt hours per year, which is roughly 1 ton of CO2 per annum reduction for these two classrooms alone.

“Both electricity consumption and peak demand were significantly reduced, resulting in lower electricity bills for the school,” said Bell.

The paint was developed by a company called ShieldCoat, which is based in Brisbane. The researchers painted it on a sample of houses, schools, offices and retail spaces.

A Mixture of Science and Art

Miller said it is a combination of the chemistry and color that makes the product effective.

“The trials indicate the economic benefits of cool roof coatings would be greatest for single-story buildings; buildings with aged, dark or medium colored roofs; buildings with no or low levels of roof insulation; and buildings with high air conditioning use,” she said.

Miller went on to say that the study revealed that the coating prevented heat from entering a building. In some cases, that led to a 30 percent reduction in air conditioning use.

The project was initiated under the Guided Innovation Alliance, which is a collaboration between the university; Ergon Energy, an electricity distributor in Queensland; and SmartGrid Partners, a Queensland-based infrastructure project management company.

Editor's Note: This article was edited at 8:45 a.m. EST to correct the temperature conversion.

   

Tagged categories: Australia; Building design; Building envelope; Building materials; Building science; Coating chemistry; Coatings Technology; Color + Design; Color selection; Colorants; Cool roof coatings; Energy efficiency; Green building; Green chemistry; Green roofs; Metal roof coatings; Reflective roof coatings; Research; Roof coatings; Roof coatings; Roofing materials

Comment from John Royal, (7/29/2015, 8:16 AM)

"The paint led to a 2-degree Celsius (35.6-degree Fahrenheit) drop in temperature to the inside areas, according to the study." This should be 3.6 degrees Fahrenheit, not 35.6.


Comment from Jill Speegle, (7/29/2015, 8:48 AM)

Thank you, John. The story has been edited to reflect the correct conversion.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
GMA Garnet USA

 
Axxiom Manufacturing

 
CRW

 
Western Technology Inc.

 
Abrasives Inc.

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
HoldTight Solutions Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us