Film, Coating Made to Protect Floors

Thursday, June 25, 2015

Comment | More

ST. PAUL, MN--3M's Scotchgard brand has updated its lineup of products to enhance protection of high-traffic floors in light industrial and commercial settings.

Scotchgard Surface Protection Film 2200 is a new offering designed to provide substantial, nearly invisible protection for building entrances, bathrooms and other areas with major foot traffic.

Scotchgard Resilient Floor Protector is a reformulation of the company's nanocoating for hospital and office floors.

Scotchgard Surface Protection Film 2200

The film is designed to reduce stripping and refinishing needs on multiple surfaces in hospitals, office buildings and other spaces.

ScotchgardSurfaceProtectionFilm2200
Photos: 3M

According to 3M, the National Floor Safety Institute certifies Scotchgard Surface Protection Film 2200 as able to provide “High Traction.

Developed to cover stone and vinyl flooring, bathroom surfaces and walls, the film helps protect against high foot traffic, furniture use and spills, according to 3M.

Available in one-, two- or four-foot squares, the film is certified by the National Floor Safety Institute as able to provide “High Traction."

The film can be used to protect waxed vinyl, sealed concrete, marble and ceramic tile terrazzo and other floor surfaces. It is compatible with standard floor cleaning procedures, disinfectants, cleaners and coatings, the company says.

More information: www.3m.com/SaveOurSurfaces.

Scotchgard Resilient Floor Protector

3M's updated Resilient Floor Protector has a zinc-free, low-odor formula that produces a hard surface.

3MResilientFloorProtector

3M's updated Resilient Floor Protector has a zinc-free, low-odor formula that produces a hard surface.

The coating offers superior gloss retention, resistance to black marks and hand sanitizers, and easier removal of black marks, according to the company.

Designed for floor maintenance in hospitals, schools, office and retail spaces, the two-coat protector is formulated for multiple surfaces, including sheet vinyl, linoleum, luxury vinyl, and Vinyl Composition Tile (VCT), the company says.

The protector works with the 3M Resilient Floor Protection System to allow for reduced chemical usage and increased operational efficiency, 3M says.

More information: www.3M.com.

   

Tagged categories: 3M; Coating Materials; Floor coatings; Floors; North America

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
WEFTEC Show

 
SAFE Systems, Inc.

 
Strategic Materials Inc.

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us