Floor Film Designed to Protect

Tuesday, June 23, 2015

Comment | More

ST. PAUL, MN--3M has created a new product designed to reduce stripping and refinishing needs on multiple surfaces in hospitals, office buildings and other spaces.

The Scotchgard Surface Protection Film 2200 has been developed to cover stone and vinyl flooring, bathroom surfaces and walls. The film will provide substantial, nearly invisible protection for areas that have high foot traffic, furniture use and spills, according to 3M.

3M

The Scotchgard Surface Protection Film 2200 is designed to reduce the number of refinishing and stripping jobs on surfaces that endure high traffic.

The surface film is available in one-, two- or four-foot squares. Ideal uses include building entrances, dining area floors, bathroom surfaces, and areas underneath chairs, the company says.

Scotchgard Surface Protection Film 2200 is certified by the National Floor Safety Institute as able to provide “High Traction,” 3M reports.

The film can be used to protect waxed vinyl, sealed concrete, marble and ceramic tile terrazzo and other floor surfaces. It’s compatible with standard floor cleaning procedures, disinfectants, cleaners and coatings, the company says.

More information: www.3m.com/SaveOurSurfaces.

   

Tagged categories: 3M; Chemical stripping; Concrete coatings and treatments; Floor coatings; Floors; Maintenance + Renovation; Maintenance coating work; North America

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
Axxiom Manufacturing

 
Seal for Life/STOPAQ

 
CRW

 
HoldTight Solutions Inc.

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Abrasives Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us