SYDNEY--Australian scientists have reportedly developed a material capable of keeping a roof cooler than the air that surrounds it, even in intense summer conditions.

The new material is billed as a “first in super-cool roof technology,” according to the team from the University of Technology Sydney (UTS).

cool roof material
Geoff Smith / Angus Gentle via UTS

Dr. Angus Gentle (pictured) and Emeritus Professor Geoff Smith of the University of Technology in Sydney have developed a roofing material that could reduce the heat island effect in urban areas.

The development has a range of benefits, including reducing the heat island effect in urban areas and peak power demand from air-conditioning, the team reports.

The scientists published their work in the journal Advanced Science.

‘Coated Polymer Stack’

The team used a mixture of commercially available polyesters and a silver layer to build what it calls a “coated polymer stack.”

The layered structure was designed to reflect strongly across the visible and some non-visible solar wavelengths.

“Roofs heat up by absorbing sunlight, so darker roofs can get very hot,” explained co-author Geoff Smith, an emeritus professor at the University of Technology.

“Even white roofs still absorb enough sunlight to warm up by 9 degrees to 12 degrees Celsius.”

During testing, the polymer stack, however, produced a surface that stayed “11 degrees (Celsius) or more colder than an existing state-of-the-art white roof nearby,” said Smith, who worked with Dr. Angus Gentle on the research.

How It Works

Applied like a coat of paint, the material mimics what happens on a roof after the sun goes down, Smith told takepart.com.

Once the sun sets, roofs made from heat-absorbing substances not only release heat back into the atmosphere, but also become cooler than the ambient temperature.

cool roof infrared
Geoff Smith / Angus Gentle via UTS

An infrared image highlights the temperature difference between the new surface (center) and an existing cool roof used in testing, the team reports.

“Our surface achieves this in the daytime,” he said, “by reflecting almost all of the incident sunlight, thus allowing the surface to remain cooler than the atmosphere.”

Smith said cooling a roof below ambient air temperature had up until now been “an elusive target.”

Performance Testing

Testing took place on the roof of a UTS science building with a clear view of the sky and no shadowing.

Data was collected for an unprotected new surface, and one aged over several days in a polluted outdoor summer environment for assessment of the impact of the build-up of dust and grime, according to the team.

Smith said the surface maintained its high performance under all conditions.

“Extensive dew formation is inevitable for a super cool roof and dew drops precipitate dirt,” he added. “This roof site being 25 meters above a busy city transit road was a stern test.”

Heat island
EPA

The Environmental Protection Agency describes "heat islands" as built-up areas that are hotter than nearby rural areas. The annual mean air temperature of a city with 1 million people or more can be 1.8–5.4°F (1–3°C) warmer than its surroundings. In the evening, the difference can be as high as 22°F (12°C).

The results revealed that “excellent thermal performance” can be achieved and maintained, he said.

More Research Underway

Moving forward, the team says it will access the cost of the material. The plastics the team selected for the prototype material are currently used in niche markets, such as small displays and mirrors for solar thermal energy, according to Smith.

Another key challenge the team faces is reducing the glare that results from the material’s highly reflective qualities, takepart.com reports.

The reflection could be a distraction to drivers and others in a densely built environment.

The study has been supported by an Australian Research Council Discovery Project grant.

   

Tagged categories: Australia; Coatings Technology; Coatings Technology; Cool roof coatings; Energy efficiency; Environmental Protection; Research; Roof coatings; Solar reflectance

Comment from Brian Hierlihy, (6/15/2015, 9:57 AM)

Strikes me that this is a health hazard for wildlife and those in surrounding, taller, buildings.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
DeFelsko Corporation

 
SAFE Systems, Inc.

 
Strategic Materials Inc.

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us