CLEVELAND--Sherwin-Williams’ Product Finishes division has introduced a new line of coating systems designed for manufacturers of prefinished wood flooring used in residential and commercial applications.
The Ultra-Cure Wood Floor Coatings line meets or exceeds key specifications for wear, scuff, scrape resistance and coating elasticity, the company reports.
 |
Sherwin-Williams |
The line includes UV-curable wood flooring coating systems, according to the company.
|
Further, Sherwin-Williams says the systems were developed to speed production and achieve consistent appearance and performance.
Applications, New Offering
The finishes are designed for use on a wide range of substrates including ceramic topcoats, high taber sealers, armor coat, fillers and sealers and UV Oil, according to product literature.
Additionally, custom color matching is available in specialized Sherwin-Williams facilities, and manufacturers will have access to proprietary color trends research and forecasting, Sherwin-Williams notes.
The coatings are the Cleveland-based company’s first entry into the North American OEM Prefinished Wood Flooring Coatings market.