Roof System Adds Low-Solids Option

Thursday, June 4, 2015

Comment | More

BROOKFIELD, WI—Volatile Free Inc. has introduced a new 70 percent solids silicone coating formulated to protect roofs from water damage and UV deterioration.

VFI-991 Silicone is a one-component, moisture-cure elastomer designed for use as a cure-in-place waterproof coating for metal, singly-ply, modified bitumen and other roof surfaces.

application of silicone roof coating
Volatile Free Inc.

VFI-991 Silicone offers protection from leaks, rust and corrosion and is UV-resistant, according to the manufacturer.

The material is the latest addition to the manufacturer’s Sealguard line, which also includes a high-solids formulation.

Features, Application

According to product literature, high-build VFI-991 Silicone is UV-resistant and offers protection from leaks, rust and corrosion.

The product is also self-flashing, the company says.

The coating can be applied by sprayer, roller or brush.

Headquartered in Brookfield, WI, Volatile Free is a manufacturer of polyurea and polyurea hybrid products and related service for the industrial and commercial roof coatings industry.

More information: www.volatilefree.com.

   

Tagged categories: Building envelope; Building Envelope; Built-up roofs (BUR); Coatings manufacturers; Metal roof coatings; North America; Roof coatings; Silicone

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
Axxiom Manufacturing

 
CRW

 
Abrasives Inc.

 
Western Technology Inc.

 
HoldTight Solutions Inc.

 
GMA Garnet USA

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us