MONETA, VA—A West Virginia contractor will be painting the 75,000-gallon water storage tank in this southern Virginia city.

Eastern Tank & Utility Services Inc., of Princeton, WV, was awarded the project with a low bid of $29,000.

Work will include cleaning and recoating the exterior of the 28-foot-wide, 75-foot-tall Boardwalk Water Storage Tank.

Moneta VA water tank bids
Owner specs via Paint BidTracker

Eastern Tank & Utility Services Inc. will clean and coat the 75,000-gallon, 75-foot-tall Boardwalk Water Story Tank in Virginia.

Others bids for the project totaled $29,970; $29,300; and $84,700.

Scope of Work

Surfaces will be prepared with an approved cleaning solvent and wiped dry. Exterior surfaces will be cleaned by low-pressure waterjet to SSPC-SP WJ 4 standards and spot power-tool cleaned to SSPC-SP 3.

Existing coatings contain lead; containment will be required.

The contractor will then apply a spot coat of acrylic primer, followed by a full prime coat of high-solids epoxy, and intermediate and finish coats of high-performance acrylic paint. Interior tank surfaces will require a controlled chlorine disinfection, to be determined by the contractor.

During cleaning, the contractor will be required to perform miscellaneous welding repairs to the tank’s appurtenances. The air vent screen will also require replacement.

The contract will also include a one-year inspection of the coating systems.

Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community.

Try PaintBidTracker free!

   

Tagged categories: Bidding; Contractors; North America; Paint BidTracker; Program/Project Management; Tanks; Waterjetting

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
CRW

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Axxiom Manufacturing

 
Abrasives Inc.

 
Sauereisen, Inc.

 
Seal for Life/STOPAQ

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us