Fruity Fiber Muffles Gypsum Alternative

Thursday, March 12, 2015

Comment | More

The task of pruning orange trees won't end out in the field if Dr. Jésus Alba has his way.

Alba and his colleagues in Spain have developed a new acoustical insulating board that incorporates fibers from orange tree pruning.

OrangeFiberTrees
RUVID

Using the pulp from discarded orange tree fibers, Spanish researchers say they have created a building board that boasts better acoustic insulation than gypsum.

Not only does the product replace new material with natural agro-waste, but the fiber-rich board provides "150% improvement" in acoustic insulation over conventional laminated gypsum, according to a research announcement by a Spanish academic consortium known as RUVID.

Alba's research team hails from the Universitat Politècnica de València and the Universitat de Girona.

The group, known by the Spanish acronym LEPAMAP, "has extensive experience in the field of compound materials strengthened with natural fibers," says Dr. Pere Mutjé of UPV.

What It Does

In the current project, raw materials for the boards come from the defibering of the pruned tree waste. The pulp-powered mix also incorporates polypropylene, the common plastic used in a wide variety of consumer products.

Acoustical testing showed that the fiber-filled boards "provide an acoustic insulation potential of about 29 dBA, and the conventional laminated gypsum boards are usually at 27 dBA," say Alba and colleague Romina del Rey.

JesusAlba
RUVID

Dr. Jésus Alba leads a team of researchers who specialize in biobased building materials.

The 2 dBA difference represents "a 50 percent improvement in the acoustic efficiency of the boards, in comparison with gypsum boards," the researchers said.

If the team sandwiches an absorbent wool between two of its boards, "the improvement is about 5 or 6 dBA, which means it will insulate more than double the conventional system," they added.

The fiber board's mechanical properties are "better than those of gypsum boards," says Alba. "...[W]ith the same board thickness, the acoustic insulation is higher...."

Alternatively, he said, a thinner fiber board can achieve the same insulation as its thicker gypsum counterpart.

Olive Pit Potential

The material meets the objectives of the European Commission's Horizon 2020, the seven-year, $84.2 billion research and innovation program, the team says.

Bisman Deu
Bisman Deu via Unicef.org

Bisman Deu (right), 16, has developed a particle board, made from husks and straw, that can withstand extreme weather conditions. Her team includes Rayvin Thingnam (left).

The research also has been published in the journal Construction and Building Materials.

Mutjé's team is now pursuing the use of ground olive pits in building materials. He calls such research "a leading example" of the current development trend in agro-waste-based building materials.

That growing field also includes green wood made from rice waste; concrete from sunflower seed husks; and new homes made from straw.

   

Tagged categories: Bio-based materials; Building Envelope; EMEA (Europe, Middle East and Africa); Green building; Gypsum board; Insulation; Renewable raw materials; Walls

Comment from William Feliciano, (3/12/2015, 8:11 AM)

Nothing is mentioned about fire resistance of the orange fiber-rich board, only sound. Gypsum board has fire ratings based on thickness I believe.


Comment from Tom Schwerdt, (3/13/2015, 8:52 AM)

Collecting, drying and processing branch trimmings is likely to be more labor and fuel intensive than simply mining gypsum or using gypsum from coal plants (flue gas desulfurization typically creates gypsum.) Still an interesting approach - I wonder what the projected costs are at commercial scale.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
Induron Coatings, Inc.

 
RCG America

 
Fischer Technology Inc.

 
HoldTight Solutions Inc.

 
DeFelsko Corporation

 
Modern Safety Techniques

 
Mitsubishi Gas Chemical America

 
SAFE Systems, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us