Aluminum Finishing Guide Gets Revamp

Monday, February 16, 2015

Comment | More

Specifiers and other building professionals have a newly updated resource on paint and anodized finishes for aluminum building components.

The American Architectural Manufacturers Association has announced an updated version of its “Anodic Finishes/Painted Aluminum” reference document—AAMA AFPA-1-15.

windows
AAMA

AAMA’s Anodic Finishes/Painted Aluminum Task Group says the reference document provides users and specifiers information on paint and anodized finishes for architectural aluminum.

The updates reflect newer technologies now involved in the anodizing process, which produce coatings that are “thicker than nature’s version, harder and very durable,” according to the association.

The document describes the appearance and physical properties of anodic finishes by three factors:

  • Aluminum alloy and temper;
  • Surface treatment before anodizing; and
  • The type of electrolyte and operating techniques used in the anodizing process.

Update Needed

“There were certain finishes that were outdated and not used in the current architectural specifications,” according to Carl Troiano, vice chair of the AMC Anodic Finishes/Painted Aluminum Task Group.

“There were tests and procedures that needed to be verified or modified, along with clarifying and identifying the specifications.

“This revision streamlined the current specification.”

AAMA AFPA 1-15 may be purchased from AAMA’s Publication Store.

AAMA offers performance standards, product certification, and educational programs for the fenestration industry. AAMA’s membership is comprised of window, door, skylight, curtain wall and storefront manufacturers, suppliers and test labs.

   

Tagged categories: AAMA; Aluminum; Anodization; Certifications and standards; Coatings Technology; Coatings Technology; Fenestration; North America; Windows

Comment from wayne vutech, (3/26/2015, 10:24 PM)

When repainting or color change is needed by a new home owner years after installation what changes would the painting contractor have to make to insure proper adhesion?


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Induron Coatings, Inc.

 
NLB Corporation

 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
Fischer Technology Inc.

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
RCG America

 
SABRE Autonomous Solutions

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us