BASF has introduced a water-based, 100 percent acrylic coating to protect vertical concrete exteriors from water and dirt.

Also suitable for concrete masonry units (CMU) and masonry, hydrophobic MasterProtect C 350 is designed to reduce exterior maintenance costs and to keep facades looking attractive.

The new coating is the latest in the MasterProtect line, which includes a range of high-performance water repellents, elastomeric and high-build anti-carbonation, chemical-resistant and corrosion-resistant coatings for concrete.

MasterProtectC350
BASF

Hydrophobic MasterProtect C 350 is designed for all vertical concrete and masonry surfaces.

The C 350 product is designed to provide long-term protection of concrete structures and steel reinforcements against the ingress of carbon dioxide, chlorides and water.

Availability, Features

Available in the U.S. and Canada, the coating can be applied as a restoration topcoat or used on new vertical construction, according to BASF. The low-VOC formulation boasts “excellent” adhesion to concrete and existing coatings, the manufacturer says.

Additional features include long-lasting color retention and resistance to wind-driven rain and heavy UV exposure, according to product data.

facades
© iStock.com / TennesseePhotographer

MasterProtect C 350 is recommended for use on concrete, masonry, stucco, EIFS and existing coatings.

MasterProtect C 350 is available in four tintbases, with formulations to match the 50 colors in the MasterProtect Color Portfolio. Custom colors are also available, BASF says.

BASF Construction Chemicals

Based in Shakopee, MN, BASF’s Construction Chemicals division manufactures chemicals for new construction, maintenance, repair and renovation of structures.

The company’s product portfolio includes waterproofing systems, sealants, concrete repair and protection systems, and performance flooring systems.

More information: www.basf.com.

   

Tagged categories: Asia Pacific; BASF; Building facades; Coating Materials; Concrete coatings and treatments; Concrete masonry units (CMU); Corrosion protection; EMEA (Europe, Middle East and Africa); Latin America; Masonry coatings; North America; Protective Coatings; Rebar

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Mitsubishi Gas Chemical America

 
KTA-Tator, Inc. - Corporate Office

 
DeFelsko Corporation

 
Fischer Technology Inc.

 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
SAFE Systems, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us