Fischer Technology's new Dualscope model features a rotating screen that automatically rights the orientation of readings and menu navigation upon changes in position.

The updated Dualscope MP0R pocket coating thickness gauge display rotates automatically to keep the readings upright, regardless of the user's position, according to the company.

Features

The gauge has an integrated probe and gives tolerance limits for upper and lower limit values.

Fischer Dualscope Dualscope
Fischer Technology

The updated Dualscope MP0R display rotates automatically to keep readings upright, the company says.

The tool also includes the company's DataCenter, software for creating, transferring, printing and archiving measurement data. IMO PSPC, SSPC-PA 2 and other specifications are installed in the gauge.

According to Fischer, typical fields of applications include powder coating, manufacturing, aero/auto industries and general metal products.

More information: www.fischer-technology.com.

   

Tagged categories: Asia Pacific; Coating / Film thickness; EMEA (Europe, Middle East and Africa); Fischer Technology; Good Technical Practice; Latin America; North America; Thickness gauge

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
DeFelsko Corporation

 
SAFE Systems, Inc.

 
Tarps manufacturing, Inc.

 
WEFTEC Show

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us