Friday, September 19, 2014

Comment | More

Cortec Corp. has introduced a heavy-duty, bio-based cleaner and degreaser for a variety of industrial and commercial jobs.

EcoClean VpCI-411 is a highly concentrated, water-dilutable D-Limonene-based cleaner/degreaser liquid with patented Vapor phase Corrosion Inhibiting technology.

Typical uses include cleaning and degreasing pipelines, tanks and vessels; removing adhesives; removing temporary coatings; and washing hands to remove oils during machine operation.

Cortec EcoClean VpCI-411
Photos: Cortec

EcoClean VpCI-411 can clean heavy-duty machinery, tools and equipment, floors, walls, lavatories and desks. It can be used on all engineering metals and alloys, according to Cortec.

According to the company, the biodegradable, environmentally safe product helps fight corrosion. The product contains 81 percent bio-based ingredients and is certified by the U.S. Department of Agriculture as a bio-based product.

Multiple Uses

EcoClean VpCI-411 is suitable for cleaning heavy-duty machinery, shop tools, hoods, parts-in-process, food processing equipment, office equipment, floors, walls, lavatories and desks. It can be used on all engineering metals and alloys, according to Cortec.

industrial cleaner/degreaser

According to the company, the biodegradable product can fight corrosion while also being environmentally safe.

It can dissolve grease, oil, paraffins and waxes and "offers a pleasant odor," the company says.

According to the company, the product is safe to handle, nontoxic and non-abrasive.

More information: www.cortecvci.com.

   

Tagged categories: Bio-based materials; Cortec; Maintenance programs; Metal cleaning; North America; Paint application equipment; Pipelines; Surface Preparation; Tanks

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
CRW

 
Seal for Life/STOPAQ

 
Abrasives Inc.

 
Tarps manufacturing, Inc.

 
HoldTight Solutions Inc.

 
Sauereisen, Inc.

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us