New ‘Bamboo’ Steel Boasts Flex Appeal

Thursday, August 7, 2014

Comment | More

Scientists have found a way to manipulate several kinds of metal to mirror the characteristics of bamboo, adding significant strength and flexibility.

The researchers at North Carolina State University and the Chinese Academy of Sciences’ Institute of Mechanics in Beijing have enhanced the metals' mechanical characteristics by modifying their internal structure to emulate bamboo.

Yuntian Zhu

Using a gradient structure on metal similar to bamboo, scientists from North Carolina State and the Chinese Academy of Sciences' Institute of Mechanics have developed stronger, more flexible metals.

“If you looked at metal under a microscope, you’d see that it is composed of millions of closely packed grains,” said Yuntian Zhu, a professor of materials science and engineering at North Carolina State and co-author of two papers on the new work, in an announcement.

“The size and disposition of those grains affect the metal’s physical characteristics.”

How it Works

Bamboo cells vary in size and density, which help give it strength and flexibility. To give metal the same characteristics, researchers gradually increased the size of the grains on the metal.

Small grains on the metal’s surface makes it harder and less ductile, meaning it can be stretched very far without breaking, according to co-author Xiaolei Wu, a professor of materials science at the Institute of Mechanics.

©Noah Bell / Bamboo Garden

The gradual interface of large and small grains makes bamboo stronger and more flexible than other materials, something researchers have mimicked in metals.

"In short, the gradual interface of the large and small grains makes the overall material stronger and more ductile, which is a combination of characteristics that is unattainable in conventional materials,” Wu said.

It also makes materials more resistant to corrosion, wear and fatigue.

The Metals

Wu and Zhu tested the gradient structure concept in a variety of metals, including copper, iron, nickel and stainless steel.

The technique improved the properties in all of them, the team said.

Wikipedia

Bridges, like this one in Portland, OR, could be made 20 percent stronger using the new gradient structure technique on steel.

The new approach was also tested on interstitial free (IF) steel, which is used in some industrial applications. IF steel is made with very low ductility, making it vulnerable to catastrophic failure.

That type of steel is generally made only strong enough to withstand 450 megapascals of stress, researchers said.

This means it can be stretched to less than 5 percent of its length without breaking, making it extremely unsafe.

Using the gradient structure approach, the IF steel was made strong enough to support 500 megapascals of stress and was able to stretch to 20 percent of its length before failing.

   

Tagged categories: Biomimicry; Bridges; Building Envelope; Building materials; Building science; Cast iron; Copper; Metals; Research; Stainless steel; Steel

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
SAFE Systems, Inc.

 
RCG America

 
DeFelsko Corporation

 
HoldTight Solutions Inc.

 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
Fischer Technology Inc.

 
AWWA (American Water Works Association)

 
Sauereisen, Inc.

 
ABKaelin, LLC

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us