Coatings Industry News

Main News Page


New Coating Repels Water Colorfully

Wednesday, June 11, 2014

Comment | More

BASF Corp.’s Wall Systems business has introduced a high-build exterior protective coating designed to repel water and resist dirt.

Tersus Color Coat expands the company's Tersus Finishes line, which rolled out a year ago.

Tersus Finishes
Photos: BASF Corp.

Tersus Color Coat is part of the Tersus Finishes line, which debuted in 2013.

Color Coat is a modified-acrylic, smooth coating formulated to produce a highly hydrophobic, non-polar surface that repels water.

"When water comes in contact with Tersus Color Coat, it beads and carries away dirt, soil and debris," BASF said in a product announcement. Its water resistance also makes the surface less vulnerable to mold and mildew.

Product Testing

Color Coat's anti-soiling properties have been successfully tested with ASTM D3719 – Dirt Collection and Miami Dade County TAS 143-95 to confirm dirt pickup resistance, according to BASF.

Tersus Color Coat

Tersus Color Coat is designed to repel water, leaving the surface better able to resist mold and mildew, according to manufacturer BASF.

“These tests enable the design professional to evaluate and ultimately specify minimum requirements of dirt collection resistance,” said Peter Daechsel, national marketing manager, BASF’s Wall Systems business.

Tersus Color Coat is available factory tinted or as a point-of-sale tint base in five-gallon pails.

More information: www.wallsystems.basf.com .

   

Tagged categories: BASF; Coatings Technology; Dirt resistance; Exterior Wall Coatings; High-build coatings; Mold/mildew-resistant coatings; Water repellents

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Induron Coatings, Inc.

 
SABRE Autonomous Solutions

 
SAFE Systems, Inc.

 
RCG America

 
NLB Corporation

 
Fischer Technology Inc.

 
DeFelsko Corporation

 
Sauereisen, Inc.

 
Modern Safety Techniques

 
HoldTight Solutions Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us