Fluoropolymer Coatings Stage Comeback

Wednesday, May 14, 2014

Comment | More

PPG Industries Inc. says it will introduce a revamped version of its Duranar ADS (air-dried system) fluoropolymer coatings this summer—three years after the products were withdrawn from the market.

According to the company’s coil and building products coatings group, the new generation of coatings for architectural metals are based on a newly formulated fluorinated copolymer resin combined with PPG proprietary chemistry.

Touch-Up Coating Product

The high-performance coatings are designed to repair fluoropolymer coatings on architectural metals damaged during production or after field installation, PPG adds.

PPG
PPG Industries

The reformulated Duranar ADS coating can be spray-applied in the field to repair or refurbish weathered metal roofing or siding panels. Duranar coatings were used on the Puerto Rico Convention Center, shown above.

The one-component formulation can be applied by fingernail brush for small touch-ups at the end of a production line or be spray-applied in the field to repair or refurbish weathered metal roofing or siding panels, according to PPG.

The new coatings will come in a wide range of color options, including solid, metallic, pearlescent and infrared-reflective (IR-reflective) pigment technologies, the company says.

More information: www.ppgideascapes.com.

   

Tagged categories: Coating chemistry; Coatings Technology; Fluoropolymer; Formulating; Metal coatings; Metals; PPG; Resins

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
PaintSquare

 
Abrasives Inc.

 
Western Technology Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us