Roller Gauges Thickness While Coating

Thursday, April 10, 2014

Comment | More

A new roller accessory from Wooster Brush allows applicators of high-performance floor and roof coatings to ensure the product’s proper mil thickness during application.

By attaching the Roller Gauge System's specially designed, polypropylene endcaps to a 3/16-inch nap roller, professionals are able to directly control the mil thickness of the coating being applied.

Roller Gauge
Photos: Wooster Brush

Controlling coating thickness during application eliminates the need for a separate squeegee process, according to Wooster Brush.

Doing so allows the applicator to eliminate the previously required squeegee process, according to Wooster.

Applications and Features

Roller Gauges can be used with floor or roof coatings such as epoxies, urethanes, anti-skid floor toppings, vapor barriers, or metallic finishes. The gauges are color-coded, with yellow for thin films (approximately 4 mils), red for medium films (approximately 12 mils), and blue for thick films (approximately 22 mils).

Each package contains six of the patent-pending endcaps.

Roller Gauge endcaps

Roller Gauge endcaps are color coded for different coating thicknesses.

Wooster Roller Gauges in yellow (R082), red (R083), and blue (R084) are available at industrial suppliers, traditional paint and decorating centers, hardware stores, and paint sundry distributors or retailers.

Founded in 1851 in Wooster, OH, The Wooster Brush Company produces more than 2,000 professional and DIY painting products.

More information: www.woosterbrush.com.

   

Tagged categories: Brushes and rollers; Coating / Film thickness; Floor coatings; Good Technical Practice; Paint application; Quality control; Roof coatings; Wooster Brush Company

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Strand’s Industrial Coatings

 
CRW

 
HoldTight Solutions Inc.

 
NLB Corporation

 
Paint BidTracker

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
Modern Safety Techniques

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us