Q-Lab Unveils 3 Corrosion Test Units

Tuesday, April 8, 2014

More items for Quality Control

Comment | More

Q-Lab, a global provider of weathering and corrosion test equipment, has introduced the Q-FOG CRH cyclic corrosion testers, designed to perform traditional salt spray, Prohesion and most cyclic automotive tests.

The Q-FOG tester allows users to cycle through "all of the most significant corrosion environments" in one chamber, the manufacturer says. Complex, multi-step test cycles can be programmed with the controller, allowing the tester to reproduce months or years of damaging conditions in days or weeks.

Q-FOG
Photos: Q-Lab

Standard test panel racks support 250 pounds; mounting grates, up to 1,200 pounds.

The unit is available in three models:

  • Base model SSP performs traditional salt spray and Prohesion tests.
  • Model CCT performs salt spray, Prohesion and most cyclic automotive tests.
  • Model CRH adds adds variable relative humidity control and an optional shower function.

Features and Characteristics

All Q-FOG chambers are available in two sizes: 600 and 1,100 liters. Test panel racks, hanging rod kits and flat grates are available for mounting specimens of all shapes and sizes weighing up to 1,200 pounds.

Caster wheel kits are available to allow for moving the units.

Q-Lab says Q-FOG testers were "specifically designed to have the lowest total cost of ownership in the industry."

Q-FOG

Q-FOG testing chambers are available in three models; each comes in two sizes.

Made of fiber-reinforced plastic, the units are easy to install, program and operate, according to Q-Lab, and can operate continuously 24/7 without supervision.

About the Company

Founded in 1956 as Q-Panel Lab Products, Q-Lab is based in Westlake, OH, with sales and distribution in 60 countries. The company is a global provider of material durability testing products and contract test services.

More information: www.q-lab.com.

   

Tagged categories: Accelerated laboratory testing; Corrosion protection; Cyclic corrosion cabinets; Q-Lab; Weathering

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
DeFelsko Corporation
 
PosiTector SHD Shore Hardness Durometer
 
PosiTector SHD measures the hardness of non-metallic materials. Features a measurement timer, auto ignore mode and internal memory. Shore A or D available.
 

 
Fischer Technology Inc.
 
Maximize Profits by Monitoring Coating Thickness
 
Learn more by contacting Fischer Technology today: 1.860.683.0781
 

 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
ARC / A.W. Chesterton Company
 
Erosion Resistant Coating
 
It’s high gloss low drag, abrasion resistant surface extends equipment life, improves material flow, enhances equipment efficiency, and reduces downtime.
 

 
SABRE Autonomous Solutions
 
Productivity
 
Personnel are free to do other tasks while the ALPHA1 does the “dirty work”.
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
SAFE Systems, Inc.
 
Portable Blast &
Recovery Equipment
 
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us