Coatings Industry News

Main News Page


PureColor Expands Wood Stain Line

Tuesday, October 8, 2013

Comment | More

PureColor Inc., a manufacturer of sustainable wood finishes, has rolled out its newest collection of wood stains.

The EvenGrain Collection is the first wood stain developed exclusively for door and millwork manufacturers, according to PureColor, based in Albuquerque, NM.

EverGrain
PureColor Inc.

The three products in the EverGrain Collection were developed exclusively for door and millwork manufacturers.

The collection consists of three products:

  • EvenGrain Woods, which "highlights the natural wood character and complexion in solid and veneered products";
  • EvenGrain HDF, which "delivers contrast on textured surfaces to simulate an authentic wood appearance and unique elements on smooth surfaces to create a Venetian Plaster-like appearance"; and
  • EvenGrain MDF, which "creates complimentary moldings and casings" for EvenGrain-finished doors.

“The EvenGrain Collection is important for door and millwork manufacturers, because it produces beautiful results on any substrate, lowers production costs, and creates new market possibilities for these producers,” said company president Scott Caruso.

The zero-VOC, no-wipe EvenGrain Collection ships and stores dry in PureColor’s “Stain in a Box” packaging and may be applied with either manual or automated equipment.

PureColor Inc. produces sustainable wood finishes for the OEM and architectural coatings market. 

More information: www.purecolorinc.com.

   

Tagged categories: Architectural coatings; Coatings manufacturers; Coatings Technology; OEM (Original Equipment Manufacturers); Wood; Wood coatings; Wood stains

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Mitsubishi Gas Chemical America

 
Induron Coatings, Inc.

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
SABRE Autonomous Solutions

 
KTA-Tator, Inc. - Corporate Office

 
Fischer Technology Inc.

 
SAFE Systems, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us