A new standard on solar reflective finishes may prove useful to architects, owners and contractors when it comes to determining the best solar reflective coating for a project, according to the American Architectural Manufacturers Association (AAMA).

The standard, AAMA 643-13, "Voluntary Specification, Performance Requirements and Test Procedures for Solar Reflective Finishes,” describes test procedures and performance requirements for pigmented organic coatings applied to aluminum and other substrates.

AAMA
AAMA

AAMA's Cool Coatings Task Group says solar reflective coatings can be used on facades, window frames, railings and other outdoor equipment enclosures.

The standard is available for purchase from AAMA’s Publication store.

Answering a Need

“Since its development, cool coatings technologies have always been thought of as being strictly for roof coatings,” said Manny Mayer, chair of AAMA’s Cool Coatings Task Group. Mayer is the architectural product manager, North America, with TIGER Drylac U.S.A. Inc., of St. Charles, IL.

“As is the case with roofs, such coatings can be beneficial on the façade as well as window frames, railings, outdoor equipment enclosures and numerous other applications as recent studies have shown,” he said.

“In order to specify such coatings for alternate purposes, AAMA’s Cool Coatings Task Group felt there was a need in the market place to provide a specification for manufacturers and architects to help in the evaluation and selection process of the best coating for the project.”

Other Architectural Substrates

In addition to aluminum, the standard covers coatings applied to fiber reinforced thermoset or wood profiles for windows, doors, wall panels and similar products.

AAMA reports that the primary purpose for utilizing coatings with solar reflective properties is to keep the coated surfaces cooler than they would be with standard coatings.

Future Use in LEED

“In order to continually meet the reduction of energy usage, AAMA 643 will help implement cool coatings technology of future projects and will be eventually used in LEED programs,” said Carl Troiano, vice chair of AAMA’s Cool Coatings Task Group. Trioiano is the president of Bay Shore, NY-based Trojan Powder Coatings Co. Inc.

Also, AAMA 643 is intended to assist the architect, owner and contractor to specify and obtain factory-applied finishes that will provide higher than standard Total Solar Reflectance values and still maintain a high level of performance in terms of film integrity, exterior durability and general appearance over a period of many years, the association said.

AAMA offers performance standards, product certification, and educational programs for the fenestration industry. AAMA’s membership is comprised of window, door, skylight, curtain wall and storefront manufacturers, suppliers and test labs.

   

Tagged categories: AAMA; Associations; Certifications and standards; Coatings technology; Energy efficiency; Fenestration; Good Technical Practice; Solar reflectance

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
HoldTight Solutions Inc.

 
Axxiom Manufacturing

 
CRW

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
Abrasives Inc.

 
Seal for Life/STOPAQ

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us