Coordinating coatings on a fast track, multi-phased project with several hundred construction workers and equipment installers on site at the same time provided a challenge for Vulcan Painters. The project, a new construction addition on an existing family-owned poultry processing business, began in cold, damp February weather, and the scope included painting all interior and exterior walls, caulking in walls and floors, and painting miscellaneous steel—piping, a sky bridge, bollards and stairways, as well as concrete masonry units (CMUs).

Eighty percent of this more than 375,000-square-foot project involved working on concrete substrates. Interior pre-cast tilt-up walls received a water-based polyurethane, and exterior tilt-up walls were sealed with a clear, breathable 100% silane, water-repellant sealer. Polyurea caulk was used as floor joint sealant. Interior CMU walls were coated with a base coat of acrylic block filler followed by multiple coats of low-VOC water-based epoxy. Exterior CMU walls were coated with a base coat of acrylic block filler followed by multiple coats of water-based semi-gloss acrylic. All coatings had the required USDA approval.


The production area’s walls were coated with a clear water-based polyurethane.

The project’s biggest challenge was coordinating coating with the work schedules of several hundred other contractor employees performing other trade work and installing equipment at the same time. That coordination required night shift work to avoid conflicts in some cases. Particularly challenging was coating in the mechanical room, a 100-foot-long and 30-foot-tall space lined with machinery, and 50 other construction workers in various trades working there at the same time. It was a tight work space for the 10-man crew. Specified materials for the project included Sherwin-Williams products, BASF items and Metzger-McGuire polyurea caulk.

By mid May, temperatures were more summer-like and painters were finishing change-order work and punch-list items. The last item to be completed was the floor joint sealant in the coolers, which had to be on and cooling at 40 degrees for two weeks before they could be caulked. The crew saw-cut the joints and installed a poly-cell backer rod prior to caulking. Metzger-McGuire caulk was selected because it can be applied at temperatures below freezing.


The mechanical room was filled with about 50 workers from other trades while Vulcan Painters worked in it.

Claims or positions expressed by sponsoring authors do not necessarily reflect the views of TPC, PaintSquare or its editors.

 

SEE ALL CONTENT FROM THIS SPONSOR

   

Advertisement

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us