TAP/CLICK TO EXPAND AD
Industrial Vacuum Equipment Corp.

Coating Protects Immersion Equipment

MONDAY, MARCH 24, 2014


A new epoxy coating offers high-temperature protection for oil and gas production equipment and other equipment operating under continuous immersion, Belzona announced.

Belzona 1523 is a two-part spray-applied epoxy coating for equipment in continuous water and hydrocarbon mixture immersion at temperatures up to 140°C (284°F).

Belzona
Belzona's new two-part spray applied epoxy coating protects equipment in high-temperature, continuous-immersion environments, the company says.
Belzona

Belzona's new two-part spray applied epoxy coating protects equipment in high-temperature, continuous-immersion environments, the company says.

The company says the coating can also withstand steam-out processes up to 210°C (410°F) and rapid depressurization.

Application Features

Quikspray, Inc.
APV Engineered Coatings

According to the company, the coating provides corrosion and chemical resistance and comes in light colors for easy inspection in dark vessels.

Applied using heated airless spray equipment, the two-coat application doesn't require flash blasting between coatings, Belzona says.

NLB Corporation
Just Like New Overspray Management

The solvent-free product can be applied in confined spaces and cures at room temperature. No separate post-cure is needed, because the product's post-cure mechanism activates at service temperatures, according to the company.

More information: www.belzona.com.

base painters
Modern Safety Techniques

Editor's Note: This article was updated March 31, 2014, at 12:15 p.m. ET to replace the product photo.

ADVERTISEMENTS

Tagged categories: Airless spray; Belzona; Coating Materials; Epoxy; Immersion service; Oil and Gas


Comments

Join the Conversation:

Sign in to add your comments.