The Future of Water Tank Interiors
The Recoating of the Norma Marshall Reservoir
From JPCL, August 2023
By Paul Trautmann and Josh Skinner, Sherwin-Williams Protective and Marine
The authors outline how a 100%-solids epoxy lining system was chosen to replace existing polyurethane- and epoxy-based linings on a 4.8-million-gallon ground storage tank, and how successful application brought the storage tank into compliance with the new NSF/ANSI/CAN 600 standard more than a year ahead of schedule....