The Importance of Hull Coating Specifications

From JPCL, April 2023

By Ralitsa Mihaylova and Carl Barnes, Safinah Group Ltd.


The authors discuss how optimal biofouling protection for ship hulls can be achieved through informed product selection and specification, controlled application and installation, monitoring and appropriate maintenance. They seek to identify optimal fouling control technologies for individual vessels by considering a variety of ship-specific factors....