Snatched from the Fire
Probing Issues with Application, Inspection and Technology Aspects of Passive Fire Protection
From JPCL, February 2023
By Mike O’Donoghue, Vijay Datta and Robin Wade, AkzoNobel
Intumescent epoxy passive fire protection has been successfully employed for almost 50 years to protect critical structures. This article highlights the factors that can be used to provide decades of prospective success for corrosion protection, weatherability and retention of the fire protection capability of epoxy PFPs....