Coatings 101: CUI Basics and Resources for Understanding It

From JPCL, February 2023


Over the past 40 years, problems with corrosion under thermal insulation have been recognized by the chemical and petrochemical industries, leading to the need for effective corrosion protection for piping, vessels and equipment. This Coatings 101 column briefly reviews how the environment for CUI is created, how piping, vessels and equipment are typically insulated, and the historical circumstances that have contributed to CUI....