No Dust, No Problem
Saving Time and Money on Concrete Sludge Tank Rehab Project
From JPCL, December 2022
By Jim Marston, Marston Industrial Services
This article goes through the steps of a project involving rehab on three concrete sludge tanks, highlighting how the four-man contracting crew was able to use sponge media abrasive to remove the existing rubberized coating and create the proper surface profile for the application of a new epoxy coating system....