Application of 100%-Solids Epoxy Helps Restore Wastewater Structures

From JPCL, October 2022

By David Adams, Warren Environmental


The author recaps a coating project with the Passaic Valley Sewerage Commission in New Jersey at one of the most extensive modern wastewater facilities in the eastern United States and the sixth largest in the country, in which 12 final clarifier tanks underwent ultra-high-pressure waterjetting before application of a high-solids epoxy system to provide long-term protection and keep the facility up and running....