Are CUI's Days Finally Numbered?
Insulative Coatings Show Potential for Eliminating Corrosion Under Insulation
From JPCL, February 2022
By Bruce Toews, Neil Wilds and Johnny C. Pourciau; Sherwin-Williams Protective & Marine
Corrosion under insulation presents a persistent problem for assets like pipes, valves, process vessels and storage tanks. This article discusses a new coating currently undergoing trials that has the potential to eliminate CUI altogether by acting as its own insulation, thus making traditional insulation obsolete....