A New Method for Testing Passive Fire Protection Coatings Performance

From JPCL, February 2022

By Richard Holliday, PPG Protective and Marine Coatings


Several recent high-profile PFP coating failures in cold-weather climates have demonstrated the need for more rigorous testing of intumescent epoxy coatings for such environments. This article highlights a comprehensive test regimen that compared five intumescent epoxy PFP products commonly specified for hydrocarbon industry steel structures....


(Login to read the full article)
   

Join the Conversation:

Sign in to our community to add your comments.