Placing the Access Platform on the Throgs Neck Bridge
From JPCL, January 2022
By Declan Farrington, Champion Painting Specialty Services Corp.
This article details the process behind the installation of what will total more than 1,223,000 square feet of suspended access platform as part of the ongoing deck replacement project on the Throgs Neck Bridge in New York City, and offers a glimpse of the cleaning and coating work yet to come....