Metalizing Alaskan Marine Structures: A Field-Friendly Method of Corrosion Protection

A Field-Friendly Method of Corrosion Protection

From JPCL, September 2021

By Ryan Wixson, TMS Metalizing Systems, Ltd.; and Cooper Curtis, Highmark Marine Fabrication, LLC


This article will outline the basics behind surface preparation and metalizing of steel structures, using specific examples of successful metalizing applications from one fabricator in Kodiak, Alaska, as proof of the results it can offer in corrosion protection....