Risky Business
Using a Risk-Based Inspection Program to Anticipate CUI Issues
From JPCL, June 2021
By Peter Bock, Performance Polymers Americas LLC
Corrosion under insulation has been an ever-present issue in the petrochemical refining industry for decades. This article will outline some of the most well-known mitigation methods and how a risk-based inspection program can help maintenance technicians plan for certain issues and have solutions ready at the helm....