Automation in Action
Options for Autonomous Surface Preparation and Coating Application
From JPCL, April 2021
By J. Peter Ault, Elzly Technology Corporation; and Rob Lanterman, KTA-Tator, Inc.
This article will examine some of the ways in which automation is being used to improve surface preparation, coating and inspection processes, highlighting several examples of currently employed technologies, including on marine ballast tanks and other industrial applications....